Galvanic Corrosion

by | Aug 24, 2012 | Plumbing, Understanding your home, Water Awareness | 0 comments

Copper to Galvanized

Today’s topic is a not so uncommon plumbing problem. While remodeling in Boise, we at Levco see all sorts of things. This problem was discovered in the utility room. The effects were carried throughout the daylight basement ceiling.

Usually, what people are really referring to when they say electrolysis is galvanic or dissimilar metal corrosion. Galvanic corrosion is caused by self-induced current created by the electrical potential of two dissimilar metals in contact with an electrolyte. The more noble metal attacks the less noble. This occurred on a recent project when two dissimilar metals, copper tube and galvanized steel pipe, were connected in the presence of an electrolyte solution also known as water.

Noble metal chart

Typically, a homeowner will go pick up some plumbing parts to fix a problem. Hey, if the threads fit together that must mean they were meant to screw together. Turns out it is a little more complicated than that. Connecting dissimilar metals, which is commonly done by accident in residential plumbing, can start a chain reaction leading to pipe failure and leaks in the less noble metal. (the galvanized pipe in this case)

One form of proper connection is called a dielectric connection. They can be purchased at most hardware stores. It keeps the metals separated by a rubber piece. Another fix is to use a brass bushing between the galvanized pipe and the copper pipe.

The smoking gun we found had a direct copper to galvanized pipe connection, a recipe for disaster. We also found copper to bronze to galvanized which is OK. When we took the ceiling down, we found a ticking time bomb (so to speak) with multiple pin holes in the galvanized pipe, which we would expect from the bad connection.

Pin Hole form Corrosion

Fixing the problem involved ripping out the down stream pipes and replacing them. In addition to the outward signs of corrosion, we also found what looked like massive mineral build up in the pipes which reduced its water carrying capacity.

Water heaters are a common place for this corrosion to occur, so they all have a sacrificial anode in them that will dissolve instead of eating a hole in the tank.

Although these principles seem obvious, they are the cause of countless headaches and occasional pipe failures. It may not be the manly thing to do to ask for plumbing advice, but make sure that when you do, it comes from a trusted, knowledgeable source.

Your comments are welcome. To ask questions or get more information about remodeling, email me directly or visit our contact page.

Disclaimer: Some of these images came from the WEB. If they are yours, and you object to them being used, please claim them and I will gladly remove and replace them at once.

Related Posts

Bringing Lead On Home To You

Bringing Lead On Home To You

Have you ever walked past a construction site where an old building was being demolished or renovated? You have likely brought some lead into your home. Have you ever gotten an old painted board or window upcycled into art?  You have likely brought some lead into your...

read more
The Circuitous Path To EPA Recognition

The Circuitous Path To EPA Recognition

Testing for Lead-based paint is easy and fun with the Lumetallix instant lead test kit. Although the 3M lead test swabs have been off the market since October 2023, we now know that 3M sold lead testing swabs to a company that will eventually reintroduce them to the...

read more

Leave A Comment

0 Comments

Submit a Comment

Your email address will not be published. Required fields are marked *

Yes, I would like to receive emails from Lead Locators. Sign me up!



By submitting this form, you are consenting to receive marketing emails from: Lead Locators. You can revoke your consent to receive emails at any time by using the SafeUnsubscribe® link, found at the bottom of every email. Emails are serviced by Constant Contact

Stay in touch

Sign up to stay in the know. We only share educational content and information. We don't believe in spam.


By submitting this form, you are consenting to receive marketing emails from: Lead Locators. You can revoke your consent to receive emails at any time by using the SafeUnsubscribe® link, found at the bottom of every email. Emails are serviced by Constant Contact

Recent Posts

Bringing Lead On Home To You

Bringing Lead On Home To You

Have you ever walked past a construction site where an old building was being demolished or renovated? You have likely brought some lead into your home. Have you ever gotten an old painted board or window upcycled into art?  You have likely brought some lead into your...

read more
The Circuitous Path To EPA Recognition

The Circuitous Path To EPA Recognition

Testing for Lead-based paint is easy and fun with the Lumetallix instant lead test kit. Although the 3M lead test swabs have been off the market since October 2023, we now know that 3M sold lead testing swabs to a company that will eventually reintroduce them to the...

read more
How Do You Quantify Lead?

How Do You Quantify Lead?

As if things weren't complicated enough. There are several ways to measure the amount of lead, and it has been driving me crazy for a while.  Not being a scientist myself, I felt compelled to dive into the answer to explain the situation we are up against in layman's...

read more
Clear And Present Danger

Clear And Present Danger

In a recent exposé on a Denver TV show, the Lumetallix lead testing product was pitted against an XRF gun to demonstrate that the XRF is a far superior tool for identifying lead hazards, essentially attempting to discredit our instant lead test by highlighting false...

read more